COLD WORK TOOL STEEL

NORM: ISO 4957

APPLICATION:

Steel susceptible to dies for pressing chemically aggressive materials, some elements of moulds for pressure die casting of the alloys of light non-ferrous metals, food industry.

CHEMICAL COMPOSITION:

CSiMnPSCrMoWVCoNi
0,33-0,45≤1,00≤1,50Max 0,030Max 0,03015,50-17,500,80-1,30---≤1,00

MECHANICAL PROPERTIES:

Hardness after Tempering ºC Symbol Value
Soft annealing HB ≤250
Toughening HB 300
Quenching with 1010 ºC in oil HRC 49
Quenching with 1010 ºC in oil and tempering

(cooling during quenching can also be gradual in the salt bath at 500–550 ºC and then in the air)

200 HRC 47
300 HRC 46
400 HRC 36.5
450 HRC 37
500 HRC 43
550 HRC 38
600 HRC 32.5

PHYSICAL PROPERTIES:

Property Unit Value
Density, ρ g*cm-3 7.6
Thermal expansion, α20-100ºC) K-1 10.4*10-6
Thermal conductivity, λ20ºC) W*m-1*K-1 26

Technological treatment processes:

Technological treatment processes Possible application Temperature, °C
Hot forming Forging + 1100-750
Rolling + 1100-750
Treatment Heat treatment Quenching + 1000-1040
Tempering + 550-650
Precipitation strengthening Supersaturation
Ageing
Annealing Soft annealing + 780-820
Stress relieving + 600-700
Thermochemical treatment Nitriding + 470-550
Other

INTERNATIONAL STEEL GRADES:

ISO CEN Russia
X38CrMo16 ISO 4957:2004 X38CrMo16 ISO 4957:2004
US Japan China