TOUGHENING AND STRUCTURAL STEEL

NORM: PN-89/H-84030/04

Anmeldung:

Steel susceptible to pins, rolls, bushings and other highly loaded elements, working at max. 150–200°C.

Chemische Zusammensetzung:

CMnSiPSCrNiMoVWTiCuInne
0,32 - 0,400,80 - 1,101,10 - 1,40Max 0,035Max 0,0351,10 - 1,40Max 0,30Max 0,10Max 0,05Max 0,20Max 0,05Max 0,25-

Mechanische Eigenschaften:

Property Symbol Unit After heat treatment
Ultimate tensile strength Rm MPa ≥ 1620
Yield stress Re (Rp0,2) MPa ≥ 1280
Elongation A % ≥ 9
Reduction of area Z % ≥ 40
Impact energy KV J ≥ 40

Technologische Verarbeitung:

Technological treatment processes Possible application Temperature, °C
Hot forming Forging + (1050 – 850)
Rolling + (1230 – 840)
Treatment Heat treatment Quenching + 860-880/o
Tempering + 500 – 650
Precipitation strengthening Supersaturation
Ageing
Annealing Normalising + (860 – 880)
Soft annealing + (680 – 720)
Thermochemical treatment Carburising
Other

INTERNATIONALE STAHLSORTEN:

ISO EN Russia
~ 35ChGSA GOST 4543 1971
US Japan China
~ 35CrMnSiA GB 3077-88